EMS-Grivory Grivory® TSG-30 PA666-GF30

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TSG-30 PA666-GF30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent flow behaviorExcellent surface finishVery good processing Application examples are stiff injection molding parts which demand excellent surface finish such as fuel tank caps, relais bearer and rear-view mirror housings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Water Absorption 6.5 %
6.5 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 110 MPa
16000 psi
conditioned; ISO 2039-1
210 MPa
30500 psi
dry; ISO 2039-1
Tensile Strength at Break 120 MPa
17400 psi
conditioned; ISO 527-1/-2
175 MPa
25400 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
conditioned; ISO 527-1/-2
9.70 GPa
1410 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
8.50 J/cm²
40.4 ft-lb/in²
conditioned; ISO 179/1eU
6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
conditioned; IEC 60243-1
25.0 kV/mm
635 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved