Material Notes:
Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) black 9922 main characteristics are the following properties: high heat aging resistanceexcellent surface finisheasy processibilityhigh stiffness and impact strength even after long-term heat tempering Grilon B XE 5026 (BG-30 H) black 9922 main attributes are to be shown for the production of parts with high needs on temperature resistance with highest demands on temperature resistance, for example parts like applications in engine rooms of vehicles.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 100 MPa
14500 psi
conditioned; ISO 2039-1
210 MPa
30500 psi
dry; ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
conditioned; ISO 527-1/-2
180 MPa
26100 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
conditioned; ISO 527-1/-2
9.50 GPa
1380 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 120 - 135 °C
248 - 275 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 37.0 kV/mm
940 kV/in
conditioned; IEC 60243-1
40.0 kV/mm
1020 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Fuel systems
Hydraulic systems
Interior
Electricals & Electronics Electrical appliances
Electrical equipment
Form Granules
Processing Injection Molding
Special Characteristics Improved heat resistance
Copyright © lookpolymers.com All Rights Reserved