Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
MD; ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 74
74
ASTM D785
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
ASTM D638
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.422 J/cm
0.790 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
253 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved