Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilizedInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-2
Flexural Strength 46.0 MPa
6670 psi
ISO 178
Flexural Modulus 3.10 GPa
450 ksi
ISO 178
Charpy Impact Unnotched 2.20 J/cm²
10.5 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75A