SABIC Innovative Plastics LNP Lubricomp ML003 PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp ML003 PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* ML003 is a compound based on Polypropylene resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa
3920 psi
50 mm/min; ISO 527
Tensile Strength, Yield 33.0 MPa
4790 psi
50 mm/min; ISO 527
Elongation at Break 21 %
21 %
50 mm/min; ISO 527
Elongation at Yield 6.5 %
6.5 %
50 mm/min; ISO 527
Tensile Modulus 1.60 GPa
232 ksi
1 mm/min; ISO 527
Flexural Strength 46.0 MPa
6670 psi
2 mm/min; ISO 178
Flexural Modulus 1.70 GPa
247 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
52.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 134 µm/m-°C

@Temperature 23.0 - 60.0 °C
74.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af