Mechanical Properties Metric English Comments
Flexural Strength 143 MPa
20700 psi
ASTM D790
PolyOne Maxxam™ MX5210-0040 RS Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 143 MPa
20700 psi
Three Point Bend
Osprey Metals CE7 Al-Si Controlled Expansion Alloy
Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Flexural Strength 143 MPa
20700 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC
LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Flexural Strength 143 MPa
20700 psi
ASTM D790
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Flexural Strength 143 MPa
20700 psi
ASTM D790
Kolon KOPA® KN3321G10V0L G/F Reinforced & Flame Retardant Nylon 66
High flame resistant, high toughness, dimensionally stableApplications A variety of connectorsInformation provided by API-Kolon.
Flexural Strength 143 MPa

@Temperature 22.0 °C
20700 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP
SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and..
Flexural Strength 143 MPa
20700 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI
LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant.
Flexural Strength 143 MPa
20700 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific)
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Strength 143 MPa
20700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS
LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant.
Flexural Strength 143 MPa
20700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
Flexural Strength 143 MPa
20700 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF002 PA 6
LNP THERMOCOMP* PF002 is a compound based on Nylon 6 resin containing 10% Glass Fiber.
Flexural Strength 143 MPa
20700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12
LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber.
Flexural Strength 143 MPa
20700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East)
Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Strength 143 MPa
20700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Flexural Strength 143 MPa
20700 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX03633C PC
LNP STAT-KON* DX03633C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Flexural Strength 143 MPa
20700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS
LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber.
Flexural Strength 143 MPa
20700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific)
LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber.
Flexural Strength 143 MPa
20700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific)
Glass filled Nylon 12
Flexural Strength 143 MPa
20700 psi
ISO 178
Polyplastics FR-PET® BLR6001MZ Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET)
Information provided by PolyPlastics.
Flexural Strength 143 MPa
20700 psi
ISO 178-93
Wellman Wellamid® MRGF1475 BK01 20% Mineral/Glass Reinforced Nylon 66
Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman.
Flexural Strength 143 MPa
20700 psi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Flexural Strength 143 MPa
20700 psi
ISO 178
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Flexural Strength 143 MPa

@Temperature 23.0 °C
20700 psi

@Temperature 73.4 °F
EN ISO 178
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Flexural Strength 143 MPa
20700 psi
ASTM D790
A. Schulman ComAlloy Comtuf® 633 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Flexural Strength 143 MPa
20700 psi
ASTM D790
SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific)
PPE+PS GF20% High Heat FR V-0