Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MRGF1475 BK01 20% Mineral/Glass Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF1475 BK01 20% Mineral/Glass Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183-87
Filler Content 20 %
20 %
Linear Mold Shrinkage, Flow 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 88.0 MPa
12800 psi
ISO 527-93
Elongation at Break 4.0 %
4.0 %
ISO 527-93
Flexural Strength 143 MPa
20700 psi
ISO 178-93
Flexural Modulus 5.25 GPa
761 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.10 kJ/m²
1.48 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-93