Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is available in all colors and is UL listed.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.83 - 2.03 g/cc
0.0661 - 0.0733 lb/in³
Molded
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 50
45 - 50
Tensile Strength 58.6 - 72.4 MPa
8500 - 10500 psi
Flexural Strength 117 - 145 MPa
17000 - 21000 psi
Flexural Modulus 11.7 - 12.4 GPa
1700 - 1800 ksi
Compressive Strength 128 - 156 MPa
18600 - 22600 psi
Izod Impact, Notched 2.67 - 3.74 J/cm
5.00 - 7.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 13.2 - 15.2 kV/mm
335 - 385 kV/in
short time
Arc Resistance >= 185 sec
>= 185 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F