Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 139 MPa | <= 20200 psi | ISO 178 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D792 |
PTS PPE/Nylon Alloy 10% Glass Filled Information provided by PTS LLC. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Strength | 139 MPa | 20200 psi | |
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs... |
|||
Flexural Strength | 139 MPa | 20200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP JX00061 PES (Europe-Africa-Middle East) LNP* Lubricomp* JX00061 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 139 MPa | 20200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D790 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Flexural Strength | 139 MPa | 20200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D790 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
Polyplastics Duranex® 304SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 139 MPa | 20200 psi | 2 mm/min; ISO 178 |
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar. |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 135 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 139 MPa | 20200 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Strength | 139 MPa | 20200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Strength | 139 MPa | 20200 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |