Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PTS PPE/Nylon Alloy 10% Glass Filled

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polyphenylene Ether, 10% Glass Filled
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS PPE/Nylon Alloy 10% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PTS LLC.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Strength 139 MPa
20200 psi
ASTM D792
Flexural Modulus 3.59 GPa
521 ksi
ASTM D792
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240.5 °C
464.9 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207.2 °C
405.0 °F
ASTM D648
Users viewing this material also viewed the following: