Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 95.86 MPa @Strain 5.77 %, Temperature -40.0 °C |
13900 psi @Strain 5.77 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 95.9 MPa @Strain 1.50 %, Temperature 40.0 °C |
13900 psi @Strain 1.50 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Stress | 96.0 MPa @Strain 13.0 %, Temperature -40.0 °C |
13900 psi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Tensile Stress | 95.5 MPa @Strain 22.7 %, Temperature -40.0 °C |
13900 psi @Strain 22.7 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 96.0 MPa @Strain 12.6 %, Temperature -40.0 °C |
13900 psi @Strain 12.6 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 96.0 MPa @Strain 13.0 %, Temperature -40.0 °C |
13900 psi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |
|||
Tensile Stress | 95.5 MPa @Strain 22.7 %, Temperature -40.0 °C |
13900 psi @Strain 22.7 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 96.0 MPa @Strain 11.0 %, Temperature -40.0 °C |
13900 psi @Strain 11.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 95.9 MPa @Strain 10.0 %, Temperature -40.0 °C |
13900 psi @Strain 10.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Stress | 95.7 MPa @Strain 5.00 %, Temperature -40.0 °C |
13900 psi @Strain 5.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |