Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 95.9 MPa @Strain 1.50 %, Temperature 40.0 °C |
13900 psi @Strain 1.50 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Stress | 95.9 MPa @Strain 10.0 %, Temperature -40.0 °C |
13900 psi @Strain 10.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |