Material Notes:
Georgia Gulf CL-7049 is a clear, high impact vinyl compound formulated for medical and food contact uses.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D-785
Tensile Strength, Yield 36.5 MPa
5300 psi
ASTM D-638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D-638
Flexural Strength 65.5 MPa
9500 psi
ASTM D-790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D-790
Izod Impact, Notched 1.07 J/cm

@Thickness 6.35 mm,
Temperature -20.0 °C
2.00 ft-lb/in

@Thickness 0.250 in,
Temperature -4.00 °F
ASTM D-256
5.34 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 21.7 J

@Temperature 23.0 °C
16.0 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 62 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Oxygen Index 32 %
32 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390°F) 190
Georgia Gulf Test