Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN®-V T150 ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®-V
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN®-V T150 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 13 g/10 min

@Load 3.80 kg,
Temperature 230 °C
13 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 39.3 MPa
5700 psi
ASTM 638
Flexural Yield Strength 58.6 MPa
8500 psi
ASTM D790
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm

@Thickness 6.35 mm
2.80 ft-lb/in

@Thickness 0.250 in
ASTM D256
1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
0.5 inch; ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
Transmission, Visible 88 %
88 %
Copyright © lookpolymers.com All Rights Reserved