Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Modulus of Elasticity | 2.20 - 6.48 GPa | 319 - 940 ksi | Average value: 4.10 GPa Grade Count:62 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Modulus of Elasticity | 2.20 - 16.5 GPa | 319 - 2390 ksi | Average value: 5.74 GPa Grade Count:64 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 2.20 - 6.00 GPa @Temperature 60.0 - 120 °C |
319 - 870 ksi @Temperature 140 - 248 °F |
Average value: 4.02 GPa Grade Count:2 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 2.20 - 2.90 GPa @Temperature 60.0 - 120 °C |
319 - 421 ksi @Temperature 140 - 248 °F |
Average value: 2.63 GPa Grade Count:1 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Modulus of Elasticity | 2.20 - 14.5 GPa | 319 - 2100 ksi | Average value: 7.24 GPa Grade Count:14 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50-8276 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 0407 Polycarbonate Suitable for extrusion, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 3859 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 5970 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 1822 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 2230 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Spartech Royalite R60M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are air.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Wanshijie APET Sheet APET sheet is one of the earliest plastic sheets our company develops and produces. It has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce .. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 21MBT621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 25MB866 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 26MB600 OPP Film Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 26MB768 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 178 |
Addiplast Addilene J 120 M20 Polypropylene Copolymer Low fluidity for extrusion or injectionInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | Conditioned; ISO 178 |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.20 - 7.20 GPa | 319 - 1040 ksi | Average value: 4.32 GPa Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Modulus of Elasticity | 2.20 - 3.45 GPa | 319 - 501 ksi | Average value: 2.96 GPa Grade Count:6 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |