Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.61 - 16.5 GPa | 669 - 2400 ksi | Average value: 9.73 GPa Grade Count:31 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 2.20 - 16.5 GPa | 319 - 2390 ksi | Average value: 5.74 GPa Grade Count:64 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 10.5 - 16.5 GPa | 1520 - 2400 ksi | Average value: 12.8 GPa Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Modulus of Elasticity | 2.77 - 16.5 GPa @Temperature -40.0 - 250 °C |
402 - 2390 ksi @Temperature -40.0 - 482 °F |
Average value: 7.45 GPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 2.77 - 16.5 GPa @Thickness 1.60 - 3.17 mm |
402 - 2390 ksi @Thickness 0.0630 - 0.125 in |
Average value: 7.45 GPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |