Modulus of Elasticity 2.20 - 6.48 GPa
319 - 940 ksi
Average value: 4.10 GPa Grade Count:62
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..