Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.930 GPa | 135 ksi | ASTM D882-02 |
NeXolve Clear Optionox® Polyimide Film/Coating Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability .. |
|||
Modulus of Elasticity | 0.930 - 13.8 GPa | 135 - 2000 ksi | Average value: 6.49 GPa Grade Count:74 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 0.931 GPa | 135 ksi | ASTM D638 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |