Mechanical Properties Metric English Comments
Modulus of Elasticity 4.48 - 14.5 GPa
650 - 2100 ksi
Average value: 8.91 GPa Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Modulus of Elasticity 4.48 - 11.0 GPa
650 - 1600 ksi
Average value: 6.01 GPa Grade Count:13
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
Modulus of Elasticity 4.48 GPa
650 ksi
3M Scotch-Weld™ DP100 FR Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi..
Modulus of Elasticity 4.48 - 13.8 GPa
650 - 2000 ksi
Average value: 6.61 GPa Grade Count:24
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..