Mechanical Properties Metric English Comments
Modulus of Elasticity 8.27 - 32.0 GPa
1200 - 4640 ksi
Average value: 13.0 GPa Grade Count:25
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Modulus of Elasticity 0.500 - 32.0 GPa

@Temperature -40.0 - 230 °C
72.5 - 4640 ksi

@Temperature -40.0 - 446 °F
Average value: 8.06 GPa Grade Count:40
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Modulus of Elasticity 12.0 - 32.0 GPa

@Temperature 60.0 - 150 °C
1740 - 4640 ksi

@Temperature 140 - 302 °F
Average value: 22.8 GPa Grade Count:1
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 14.0 - 32.0 GPa

@Temperature 150 - 250 °C
2030 - 4640 ksi

@Temperature 302 - 482 °F
Average value: 23.3 GPa Grade Count:2
Overview of materials for Epoxy Molding Compound