Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 10%Glass Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh quality terminal bar, switches and plugs, relais, lamp reflectors, sterilizable medical equipment.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.59 g/cc
1.59 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Stress 140 MPa
20300 psi
Elongation at Yield 2.0 %
2.0 %
2.5 %
2.5 %
flexural
Modulus of Elasticity 12.0 GPa
1740 ksi
Flexural Strength 200 MPa
29000 psi
Flexural Modulus 10.0 GPa
1450 ksi
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
CTE, linear 33.0 µm/m-°C
18.3 µin/in-°F
DIN 53752
Thermal Conductivity 0.380 W/m-K
2.64 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 180 °C
356 °F
200 °C
392 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 350 °C
662 °F
mass temp
Nozzle Temperature 340 - 360 °C
644 - 680 °F
Zone 1 355 - 375 °C
671 - 707 °F
Zone 2 360 - 380 °C
680 - 716 °F
Zone 3 350 - 370 °C
662 - 698 °F
Mold Temperature 120 - 200 °C
248 - 392 °F
Drying Temperature 150 °C

@Time 10800 - 18000 sec
302 °F

@Time 3.00 - 5.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (beige)