Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 70.0 GPa | >= 10200 ksi | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | 70.3 GPa | 10200 ksi | |
Mateck Laser Grade Zinc Selenide, ZnSe CVD Optical Crystals |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | Young's Modulus |
Momentive Performance Materials Type 254 Fused Quartz Tubing A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen .. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Schott N-ZK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | Typical |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | Transverse |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Alcoa QC-10® Aluminum Mold Alloy Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Alcoa Toolrite 2011®-T3 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Alcoa Toolrite 2011®-T4 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Alcoa Toolrite 2011®-T8 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Modulus of Elasticity | 70.3 GPa | 10200 ksi | |
Aleris Hokotol Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX PLANAL 6082 T651 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Modulus of Elasticity | 70.3 GPa | 10200 ksi | |
Aleris Hokotol Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Modulus of Elasticity | 70.3 GPa | 10200 ksi | |
Aleris Hokotol Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Modulus of Elasticity | 70.3 GPa | 10200 ksi | |
Aleris Hokotol Aluminum Alloy, 325 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX 2017A T451 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then naturally aged. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX 5083 O/H111Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX 6082 T651 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX ACP 5080 Aluminum Cast Plate ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
Teijin Technora® Fiber Technora® is a Teijin registered trademark. |
|||
Modulus of Elasticity | 70.0 GPa | 10200 ksi | |
ALIMEX ACP 5080R Aluminum Cast Material Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information .. |