Lubrizol Estane® ALR E60D Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR E60D Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR E60D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 57.2 MPa
8300 psi
ASTM D412
Elongation at Break 360 %
360 %
ASTM D412
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D412
200% Modulus 0.0207 GPa
3.00 ksi
ASTM D412
300% Modulus 0.0414 GPa
6.00 ksi
ASTM D412
Flexural Modulus 0.255 GPa
37.0 ksi
ASTM D790