Axiall 19890 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 19890 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Highly recommended for 105°C, 15 mil wall insulations and jackets where good gasoline and oil resistance is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.48 g/cc
1.44 - 1.48 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 86 - 92
86 - 92
delayed; ASTM D-2240
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Elongation at Yield 275 %
275 %
ASTM D-638
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F