Axiall 22912 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 22912 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-lead stabilized, 75C rated jacket compound suitable for CM, CL2 constructions over HDPE primaries. Also suitable for riser applications over FR PVC primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.41 g/cc
1.37 - 1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 94
88 - 94
delayed; ASTM D-2240
Tensile Strength, Yield 19.7 MPa
2850 psi
ASTM D-638
Elongation at Yield 266.6 %
266.6 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
320 %
320 %
ASTM D-638
100% Modulus 0.0152 GPa
2.20 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 31.5 %
31.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F