Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D-638 |
Plaskolite Optix® CA - 900 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D638 |
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet) |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D412 |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D638 |
Quantum PBT Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 55.2 - 68.9 MPa | 8000 - 10000 psi | ASTM D638 |
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | |
Indium Corp. Indalloy® 261 Bismuth-Silver Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill FR® PC FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection Molding Appearance: Clear/TransparentInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D638 |
Teknor Apex Chemlon® 267 Nylon 6, Impact Modified Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good .. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D412 |
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill FR® PC FR RD064 Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: RedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | >= 55.2 MPa | >= 8000 psi | |
Master Bond UV24TKLO One Component, UV-Curable, Low Outgassing Adhesive System Master Bond Polymer System UV24TKLO is a one part UV curable epoxy modified formulation for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-5.. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D638 |
Ensinger Tecapeek® XP-97 Compression Molded PEEK Compound, 30% Graphite Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 55.2 - 68.9 MPa | 8000 - 10000 psi | |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Tensile Strength | 55.2 - 68.9 MPa | 8000 - 10000 psi | |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Tensile Strength | 55.2 MPa | 8000 psi | ASTM D-638 |
Plaskolite West Optix® CA - 900 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |