Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Chemlon® 267 Nylon 6, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Teknor Apex Company
Trade Name Chemlon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Chemlon® 267 Nylon 6, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good Processability; Good Toughness; High Strength Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 1.3 %
1.3 %
24 hr; ASTM D750
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Temperature 22.8 °C
4.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 210 °C
410 °F
Users viewing this material also viewed the following: