Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 55.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 55.2 MPa
8000 psi
ASTM D-638
Plaskolite Optix® CA - 900 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet)
Tensile Strength 55.2 MPa
8000 psi
ASTM D412
Northstar Polymers MPP-D80B Rigid Polyurethane
MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus..
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Quantum PBT
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 55.2 - 68.9 MPa
8000 - 10000 psi
ASTM D638
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Tensile Strength 55.2 MPa
8000 psi
Indium Corp. Indalloy® 261 Bismuth-Silver Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Techmer ES HiFill FR® PC FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection Molding Appearance: Clear/TransparentInformation provided by TP Composites, Inc.
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Teknor Apex Chemlon® 267 Nylon 6, Impact Modified
Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good ..
Tensile Strength 55.2 MPa
8000 psi
ASTM D412
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane
Features: - Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility a..
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Techmer ES HiFill FR® PC FR RD064
Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: RedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength >= 55.2 MPa
>= 8000 psi
Master Bond UV24TKLO One Component, UV-Curable, Low Outgassing Adhesive System
Master Bond Polymer System UV24TKLO is a one part UV curable epoxy modified formulation for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-5..
Tensile Strength 55.2 MPa
8000 psi
ASTM D638
Ensinger Tecapeek® XP-97 Compression Molded PEEK Compound, 30% Graphite Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 55.2 - 68.9 MPa
8000 - 10000 psi
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound
BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Tensile Strength 55.2 - 68.9 MPa
8000 - 10000 psi
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
Tensile Strength 55.2 MPa
8000 psi
ASTM D-638
Plaskolite West Optix® CA - 900 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Tensile Strength 55.2 MPa
8010 psi
Henkel Hysol EA 9396 Paste Adhesive System
Two-part, low viscosity, unfilled version of Hysol EA 9394. Qualified to BMS 8-301.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding
Copyright © lookpolymers.com All Rights Reserved