Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 7500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 51.7 MPa
7500 psi
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4..
Tensile Strength 51.7 MPa
7500 psi
ASTM D638
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade
Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Tensile Strength 51.7 MPa
7500 psi
ASTM D638
Techmer ES Elastoblend® PA6/6 IM X Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP..
Tensile Strength >= 51.7 MPa
>= 7500 psi
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy
Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera..
Tensile Strength >= 51.7 MPa
>= 7500 psi
Master Bond EP21NDLO Low Outgassing, Room Temperature Curing Two Component Epoxy
Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21ND-LO has a convenient one to one mix r..
Tensile Strength 51.7 MPa
7500 psi
ASTM D412
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Tensile Strength 51.7 MPa

@Temperature 75.0 °C,
Time 0.000 sec
7500 psi

@Temperature 167 °F,
Time 0.000 hour
30 mil sheet, Immersion in Water
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Tensile Strength >= 51.7 MPa
>= 7500 psi
Master Bond EP30QF Quartz Filled, Two Component Epoxy System
Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at..
Tensile Strength >= 51.7 MPa
>= 7500 psi
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy
Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs..
Tensile Strength 51.7 MPa
7500 psi
ASTM D638
Ensinger Tecapeek® XP-113 Compression Molded PEEK Compound, 10% PTFE, 15% Graphite, and 3% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 51.7 MPa
7500 psi
ASTM D638
Ensinger Tecapeek® XP-93 Compression Molded PEEK Compound, 30% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 51.7 MPa
7500 psi
Cross; ASTM D882
Arlon DiClad 880 PTFE/Woven Fiberglass Laminate
Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch..
Tensile Strength 51.7 MPa
7500 psi
ASTM D412
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai..
Tensile Strength 51.7 MPa
7500 psi
ASTM D412
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat..
Tensile Strength >= 51.7 MPa
>= 7500 psi
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..
Copyright © lookpolymers.com All Rights Reserved