Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating

Category Polymer , Film , Thermoplastic , Poly (P-Xylylene)
Manufacturer Specialty Coating Systems (SCS)
Trade Name Parylene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 450°C) and those in which long-term UV stability is required. Parylene HT also has a low coefficient of friction and dielectric constant, and a high penetrating ability.SCS Parylene conformal coatings are ultra-thin, pinhole-free polymer coatings that provide a number of high-value surface treatment properties such as excellent moisture, chemical and dielectric barrier properties, thermal and UV stability, and dry-film lubricity. Parylene coatings are used in a number of applications throughout the medical device, electronics, automotive, military and aerospace industries.Information provided by Specialty Coating Systems (SCS) .
Physical Properties Metric English Comments
Water Vapor Permeability 0.220 g mil/ (m2 day)

@Temperature 38.0 °C
0.0142 g mil/ (100 in2 day)

@Temperature 100 °F
100% RH; ASTM F1249
Density 1.32 g/cc
0.0477 lb/in³
ASTM D1505
Water Absorption <= 0.010 %

@Time 86400 sec
<= 0.010 %

@Time 24.0 hour
ASTM D570
Oxygen Transmission 23.5 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
59.7 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Nitrogen Transmission 4.80 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
12.2 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Carbon Dioxide Transmission 95.4 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
242 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength 51.7 MPa
7500 psi
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D882
Elongation at Break <= 200 %
<= 200 %
ASTM D882
Elongation at Yield 2.0 %
2.0 %
ASTM D882
Modulus of Elasticity 2.55 GPa
370 ksi
Secant; ASTM D5026
Coefficient of Friction, Dynamic 0.13
0.13
ASTM D1894
Coefficient of Friction, Static 0.15
0.15
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C
20.0 µin/in-°F
via TMA
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Thermal Conductivity 0.0960 W/m-K
0.666 BTU-in/hr-ft²-°F
ASTM 1461
Melting Point >= 500 °C
>= 932 °F
via DSC
Maximum Service Temperature, Air 350 °C
662 °F
Continuous; ASTM 5026
450 °C
842 °F
Short Term; ASTM 5026
Softening Point 377 °C
711 °F
T5 Point; modulus = 690 MPa (100,000 psi)
>= 450 °C
>= 842 °F
T4 point; modulus = 70 MPa (10,000 psi)
Optical Properties Metric English Comments
Refractive Index 1.559
1.559
n<sub>D</sub>; ASTM D542
Transmission, Visible 88 %

@Wavelength 400 nm
88 %

@Wavelength 400 nm
UV Transmittance <= 1.0 %

@Wavelength 273 nm
<= 1.0 %

@Wavelength 273 nm
cutoff
80 %

@Wavelength 300 nm
80 %

@Wavelength 300 nm
88 %

@Wavelength 350 nm
88 %

@Wavelength 350 nm
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
50% RH; ASTM D257
Surface Resistance 5.00e+15 ohm
5.00e+15 ohm
50% RH; ASTM D257
Dielectric Constant 2.17

@Frequency 1.00e+6 Hz
2.17

@Frequency 1.00e+6 Hz
ASTM D150
2.2

@Frequency 1000 Hz
2.2

@Frequency 1000 Hz
ASTM D150
2.21

@Frequency 60.0 Hz
2.21

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 213 kV/mm
5400 kV/in
ASTM D149
Dissipation Factor <= 0.00020

@Frequency 60.0 Hz
<= 0.00020

@Frequency 60.0 Hz
ASTM D150
0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
ASTM D150
0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
Compliance Properties Metric English Comments
USP Class VI Yes
Yes
Descriptive Properties Value Comments
Biocompatibility ISO 10993