Polymer Property : Tensile Strength = 59.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 45.5 - 59.3 MPa
6600 - 8600 psi
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound
BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe..
Tensile Strength 45.5 - 59.3 MPa
6600 - 8600 psi
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos..