Aaron Industries AAROPRENE® AEN 6600-3 Nylon 6/6 Engineered Resin

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® AEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® AEN 6600-3 Nylon 6/6 Engineered Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 45.5 MPa
6600 psi
ASTM D638
Flexural Modulus 1.64 GPa
238 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 199 °C
390 °F
ASTM D648