Polymer Property : Tensile Strength = 10200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 70.0 - 390 MPa
10200 - 56600 psi
MD
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic
Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Quantum Polysulfone
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Injection; ISO 527
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Injection and Compression; ISO 527
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or ..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)  (Unverified Data**)
Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)  (discontinued **)
Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)  (Unverified Data**)
Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)  (discontinued **)
Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo..
Tensile Strength 70.6 MPa
10200 psi
50 mm/min; ISO 527-1,-2
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 70.0 MPa
10200 psi
DIN 53455
Isoflon POM H Polyacetal H
Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon.
Tensile Strength 70.3 MPa

@Thickness 3.18 mm
10200 psi

@Thickness 0.125 in
ASTM D638
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU)
Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr..
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro..
Tensile Strength 70.0 MPa
10200 psi
dry; ISO 527
Ter Hell Plastic Terez® PA/PP 7500 GF 7/1 Polyamide/Polypropylene
Medium viscosity special compound with increased rigidity and low moisture absorption.Application: For molding parts with high mechanical requirements at low moisture absorption.Information provide..
Tensile Strength 70.0 MPa

@Temperature 23.0 °C
10200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP..
Tensile Strength >= 70.0 MPa
>= 10200 psi
IEC 1212-2 5.7
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe.
Tensile Strength >= 70.0 MPa
>= 10200 psi
IEC 1212-2 5.7
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe.
Tensile Strength >= 70.0 MPa
>= 10200 psi
IEC 1212-2 5.7
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet
Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe.
Tensile Strength >= 70.0 MPa
>= 10200 psi
IEC 1212-2 5.7
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet
Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid..
Tensile Strength 70.0 MPa
10200 psi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced
30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Tensile Strength 70.0 MPa
10200 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Tensile Strength 70.0 MPa

@Strain 10.0 %,
Temperature 0.000 °C
10200 psi

@Strain 10.0 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
BASF Elastollan R 1000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength >= 70.0 MPa
>= 10200 psi
IEC 1212-2 5.7
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet
Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Compression; ISO 527
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Tensile Strength 70.0 MPa
10200 psi
ISO R527, 5 mm/min
Lucite International SW Sanitary Ware Acrylic Sheet
Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International