Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)  (Unverified Data**)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withstands prolonged exposure to high temperatures and repeated sterilization. Udel P-1710 polysulfone is highly resistant to mineral acids, alkali and salt solutions. Its resistance to detergents and hydrocarbon oils is good, but it will be attacked by polar solvents such as ketones, chlorinated hydrocarbons and aromatic hydrocarbons. The resin is also highly resistant to degradation by gamma or electron beam radiation. Electrical properties are stable over a wide temperature range and after immersion in water or exposure to high humidity. - Natural: Udel P-1710 NT 15Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 343 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Elongation at Break 50 - 100 %
50 - 100 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Strength 106 MPa
15400 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
ASTM D150
3.14

@Frequency 1000 Hz
3.14

@Frequency 1000 Hz
ASTM D150
3.15

@Frequency 60.0 Hz
3.15

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0011

@Frequency 60.0 Hz
0.0011

@Frequency 60.0 Hz
ASTM D150
0.0013

@Frequency 1000 Hz
0.0013

@Frequency 1000 Hz
ASTM D150
0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 329 - 385 °C
624 - 725 °F
Mold Temperature 121 - 163 °C
250 - 325 °F
Drying Temperature 135 - 163 °C
275 - 325 °F
Dry Time 3.50 hour
3.50 hour
Shot Size 50 - 75 %
50 - 75 %
Descriptive Properties Value Comments
Agency Ratings NSF 61
Tested at 82 °C (180 °F) (Commercial Hot)
Appearance Colors Available
Opaque
Availability Asia Pacific
Europe
North America
South America
Features Acid Resistant
Alcohol Resistant
Alkali Resistant
Good Chemical Resistance
Good Dimensional Stability
Good Toughness
High Heat Resistance
Hydrocarbon Resistant
Hydrolytically Stable
Forms Pellets
Generic PSU
Processing Method Extrusion
Film Extrusion
Injection Molding
Pipe Extrusion
Profile Extrusion
Sheet Extrusion
RoHS Compliance RoHS Compliant
Uses Appliance Components
Appliances
Electrical Parts
Electrical/Electronic Applications
Fittings
Food Service Applications
Industrial Parts
Microwave Cookware
Piping
Plumbing Parts
Valves/Valve Parts