Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 70.0 - 390 MPa | 10200 - 56600 psi | MD |
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co.. |