Ter Hell Plastic Terez® PA/PP 7500 GF 7/1 Polyamide/Polypropylene

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PA/PP 7500 GF 7/1 Polyamide/Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium viscosity special compound with increased rigidity and low moisture absorption.Application: For molding parts with high mechanical requirements at low moisture absorption.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 1183
Water Absorption 5.7 %
5.7 %
ISO 62
Moisture Absorption at Equilibrium 1.8 %
1.8 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
dry; ISO 527
Tensile Strength 70.0 MPa
10200 psi
dry; ISO 527
Tensile Strength, Yield 75.0 MPa
10900 psi
dry; ISO 527
Elongation at Break 5.0 %
5.0 %
dry; ISO 527
Elongation at Yield 3.0 %
3.0 %
dry; ISO 527
Tensile Modulus 3.90 GPa
566 ksi
dry; ISO 527
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ISO 75
Vicat Softening Point 160 °C
320 °F
B 120; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Processing Temperature 230 - 270 °C
446 - 518 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour