Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 100 MPa | 14500 psi | ASTM D-638 |
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material SYRON™ 7000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7000 is thermally stable, with a .. |
|||
Tensile Strength | 100 MPa | 14500 psi | RT; ASTM D638 |
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ISO 527 |
Panjin Zhongrun Chemerize 085P Low Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Tensile Strength | 100 - 120 MPa | 14500 - 17400 psi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Tensile Strength | 100 MPa | 14500 psi | 51 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta.. |
|||
Tensile Strength | 100 MPa @Temperature 23.0 °C |
14500 psi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |
|||
Tensile Strength | 100 MPa | 14500 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Tensile Strength | 100 MPa | 14500 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Techmer ES HiFill FR® TPX-PBT-00014 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Tensile Strength | 100 MPa @Thickness >=1.50 mm |
14500 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera.. |
|||
Tensile Strength | 100 MPa @Thickness >=1.50 mm |
14500 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Tensile Strength | 100 MPa | 14500 psi | cond.; DIN 53 455 |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Tensile Strength | >= 100 MPa | >= 14500 psi | IEC 1212-2 5.7 |
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.Information provided by Hippe. |
|||
Tensile Strength | >= 100 MPa | >= 14500 psi | IEC 1212-2 5.7 |
Hippe PF CP 203 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Tensile Strength | 100 MPa | 14500 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Tensile Strength | 100 MPa | 14500 psi | ASTM D638 |
Applied Nanostructured Solutions Carbon NanoStructure Chopped Fiber Carbon NanoStructure (CNS) Chopped Fiber begins as a single-end glass roving product, such as E-CR glass, that is enhanced using a proprietary ANS process. Unique multiwall carbon nanotube-based CNS.. |
|||
Tensile Strength | >= 100 MPa | >= 14500 psi | IEC 1212-2 5.7 |
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe. |
|||
Tensile Strength | 100 - 120 MPa | 14500 - 17400 psi | Injection; ISO 527 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Tensile Strength | 100 MPa | 14500 psi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF10 GB20 Polyamide 6 - Glass Beads Reinforced 10% Glass fiber and 20% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Tensile Strength | 100 MPa | 14500 psi | ISO 527 |
Panjin Zhongrun Chemerize 021G Medium Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Tensile Strength | 100 MPa | 14500 psi | ISO 527 |
Panjin Zhongrun Chemerize 021P Medium Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Tensile Strength | 100 MPa | 14500 psi | ISO 527 |
Panjin Zhongrun Chemerize 085G Low Viscosity CoPEEK Information provided by Bieglo Gmbh. |