Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole

Category Polymer , Thermoplastic , Polybenzimidazole (PBI)
Manufacturer PBI Performance Products, Inc.
Trade Name Celazole®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. Celazole® T-Series products combine the superior mechanical properties and thermal resistance of PBI with the melt process ability of polyaryletherketones.Designed for injection molding and extrusionTU-60 is a high performance unfilled blend, ideal for applications requiring no fillers. This material works well for complex geometries and offers the best process ability. Ideal for lamp sockets, connectors and back up seals.Information provided by PBI Performance Products
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Moisture Absorption at Equilibrium 6.5 %
6.5 %
ASTM D570
Loss On Ignition 5.0 %

@Temperature 499 °C
5.0 %

@Temperature 930 °F
Air; ASTM TGA
5.0 %

@Temperature 499 °C
5.0 %

@Temperature 930 °F
Nitrogen; ASTM TGA
Mechanical Properties Metric English Comments
Hardness, Rockwell A 25
25
ASTM D785
Tensile Strength 100 MPa
14500 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
Tensile Modulus 5.00 GPa
725 ksi
Flexural Strength 175 MPa
25400 psi
ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
Compressive Strength 206 MPa
29900 psi
ASTM D695
Compressive Modulus 2.90 GPa
421 ksi
Thermal Properties Metric English Comments
CTE, linear 34.0 µm/m-°C

@Temperature 25.0 - 150 °C
18.9 µin/in-°F

@Temperature 77.0 - 302 °F
ASTM TMA
70.0 µm/m-°C

@Temperature 200 - 300 °C
38.9 µin/in-°F

@Temperature 392 - 572 °F
ASTM TMA
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1000 Hz
3.4

@Frequency 1000 Hz
ASTM D150
3.4

@Frequency 10000 Hz
3.4

@Frequency 10000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 10000 Hz
0.0010

@Frequency 10000 Hz
ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495