Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet

Category Polymer , Thermoset , Phenolic , Phenolic/Glass Fiber SMC
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.60 - 1.80 g/cc
1.60 - 1.80 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 100 MPa
>= 14500 psi
IEC 1212-2 5.7
Flexural Strength >= 140 MPa
>= 20300 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 14.0 GPa
>= 2030 ksi
IEC 1212-2 5.2
Izod Impact, Unnotched (ISO) >= 29.0 kJ/m²
>= 13.8 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 2.50 J/cm²
>= 11.9 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+8 ohm
>= 1.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.0

@Frequency 48.0 - 62.0 Hz
<= 5.0

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 20000 V

@Temperature 90.0 °C
>= 20000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Comparative Tracking Index >= 100 V
>= 100 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 120 T.I.
IEC 1212-2 7.1
Water Absorption < 310 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm