Permabond ET505 Epoxy Resin

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond ET505 Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET505 forms tough bonds providing high peel resistance and high shear strength. The extended work life of this product allows for adjustment and makes it more suitable for larger applications. Features & Benefits: Adhesion to a wide variety of substrates Full cure at room temperature Easy to apply High shear and peel strength Good impact strength Good chemical resistance Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ET505B, Amine Hardener
1.17 g/cc
1.17 g/cc
ET505A, Epoxy Resin
Viscosity 17500 cP

@Temperature 25.0 °C
17500 cP

@Temperature 77.0 °F
ET505B, Amine Hardener
20000 cP

@Temperature 25.0 °C
20000 cP

@Temperature 77.0 °F
ET505A, Epoxy Resin
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
Elongation at Break 10 %
10 %
Adhesive Bond Strength 18.0 - 21.0 MPa
2610 - 3050 psi
Mild steel, Shear
Peel Strength 2.40 - 3.20 kN/m
13.7 - 18.3 pli
ISO 4578
Thermal Properties Metric English Comments
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 50.0 °C
122 °F
Processing Properties Metric English Comments
Cure Time 120 - 180 min
2.00 - 3.00 hour
handling time
4320 min
72.0 hour
full cure
Pot Life 60.0 - 120 min

@Temperature 20.0 °C
60.0 - 120 min

@Temperature 68.0 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Amber for Amine Hardener
Colorless for Epoxy Resin
Maximum Gap Fill (mm) 2
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C