Permabond UV620 UV-curable Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond UV620 UV-curable Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. It is well suited for a variety of applications including glass furniture, decorative ornaments and other glass objects where high strength and appearance are required. Features & Benefits: Cure on demand Optically clear  Resistant to yellowing Fast curing with low-power lamps 100% solids, no solvents Excellent adhesion to metal and glass Information provided by Permabond.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
uncured
Viscosity 2000 - 3000 cP

@Temperature 25.0 °C
2000 - 3000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
Tensile Strength 16.0 MPa
2320 psi
ASTM D2095
Elongation at Break 75 %
75 %
Adhesive Bond Strength 9.00 - 10.0 MPa
1310 - 1450 psi
Glass/steel, Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
4.0

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Strength 12.0 kV/mm
305 kV/in
Processing Properties Metric English Comments
Cure Time 0.0833 min
0.00139 hour
fixture time, (low power 4mW lamp)
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Colorless, clear
Uncured
Cure Wavelength (nm) 365-400
Maximum Gap Fill (mm) 1.5
Strength Retention 10% at 200°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 150°C
Relative to 0°C
75% at 100°C
Relative to 0°C
95% at 50°C
Relative to 0°C