Material Notes:
Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with metal parts (as in a threaded pipe joint). The product is instant sealing with full cure occurring in 12-16 hours. The permanent seal is inert to hydrocarbons (gasoline, diesel fuel), most acids, solvents and steam. Permabond® LH054 seals iron, copper or brass pipe and is designed to obtain more complete cure on less active surfaces such as stainless steel and aluminum. The product is available in a brush-top dispenser. It is applied onto the first few threads, assembled and tightened with a wrench. Instant sealability of 500 psi is obtained, but final adjustment can be made up to several hours after assembly. Features & Benefits: Easy to use and apply Directional freedom Does not contain solvents Excellent chemical and temperature resistance Cures at room temperature Will not shred, tear or cause blockages Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 260000 cP

@Temperature 25.0 °C
260000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.00 MPa
1020 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 360 - 960 min

@Temperature 23.0 °C
6.00 - 16.0 hour

@Temperature 73.4 °F
M10 steel, handling strength
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 20% at 200°C
Relative to 0°C
60% at 150°C
Relative to 0°C
85% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 2
M10 steel, prevail
3
M10 steel, break
UV Fluorescence No
Uncured