Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Solids Content 57.7 %
57.7 %
by volume
69.9 %
69.9 %
by weight
Volatile Organic Compounds (VOC) Content 431 g/l
431 g/l
Viscosity 400 - 600 cP
400 - 600 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
43.9 microns
1.73 mil
estimated wet film thickness
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 316 °C
600 °F
Continuous
427 °C
800 °F
Intermittent
Flash Point 47.8 °C
118 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Touch
2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
1.0 - 24.0 hour
1.0 - 24.0 hour
Recoat
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
45.0 min

@Temperature 249 °C
0.750 hour

@Temperature 480 °F
60.0 min

@Temperature 232 °C
1.00 hour

@Temperature 450 °F
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F.
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Black
Dry Film Coverage ft2/gal 925
at 1 mil
Primer Not Required
Thinner PM Acetate