Material Notes:
Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.Information provided by Imerys
Physical Properties Metric English Comments
Bulk Density 0.705 g/cc
0.0255 lb/in³
loose
1.12 g/cc
0.0405 lb/in³
packed
Brightness 94 %
94 %
Dry Brightness (Green Filter)
Particle Size 5.0 µm
5.0 µm
19% finer than
10 µm
10 µm
40% finer than
12 µm
12 µm
mean
20 µm
20 µm
72% finer than
30 µm
30 µm
87% finer than
Particle Mesh Size 20 Mesh
20 Mesh
0% retained
30 Mesh
30 Mesh
0% retained
40 Mesh
40 Mesh
0% retained
100 Mesh
100 Mesh
trace retained
140 Mesh
140 Mesh
trace retained
170 Mesh
170 Mesh
0.1% retained
200 Mesh
200 Mesh
0.3% retained
325 Mesh
325 Mesh
3.6% retained
pH 8.7
8.7
Specific Surface Area 0.90 - 1.2 m²/g
0.90 - 1.2 m²/g
Mechanical Properties Metric English Comments
Hardness, Mohs 6.0 - 6.5
6.0 - 6.5
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
Component Elements Properties Metric English Comments
Al2O3 18.5 %
18.5 %
CaO 1.5 %
1.5 %
Fe2O3 0.060 %
0.060 %
K2O 4.1 %
4.1 %
Loss on Ignition(%) 0.30 %
0.30 %
Na2O 6.5 %
6.5 %
SiO2 68.6 %
68.6 %
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %