Formosa Plastics Formolon® 265 PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 265 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Copolymer Blending Resin F-265 is a fine particle size polyvinyl chloride vinyl acetate copolymer plastisol blending resin. The product has been designed for use in application where rapid gelation and fusion is a requirement, due to low processing temperatures. When used in combination with copolymer dispersion resin, F-265 has been successfully used in carpet backing, automotive sealants and underbody coatings as well as walk-off mats.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Volatiles 0.30 %
0.30 %
ASTM D3030
Particle Size 35 µm
35 µm
Average; Coulter Counter LS230
Particle Mesh Size 40 Mesh
40 Mesh
100% thru; ASTM D1921B
270 Mesh
270 Mesh
97% thru; ASTM D1921B
Viscosity 0.85 cP
0.85 cP
Inherent; ASTM D1243
Relative Viscosity 1.95 cP
1.95 cP
QC-10-104
Vinyl Acetate Content 5.0 %
5.0 %
QC-10-105
Descriptive Properties Value Comments
K-Value 63
Fikentscher's Constant