Imerys Minsilsparâ„¢ Feldspar

Category Ceramic , Clay , Feldspar Clay , Oxide , Silicon Oxide
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Minsilspar™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Minsilsparâ„¢ Feldspar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys
Physical Properties Metric English Comments
Bulk Density 0.833 g/cc
0.0301 lb/in³
loose
1.33 g/cc
0.0480 lb/in³
packed
Brightness 91 %
91 %
Dry Brightness (Green Filter)
Particle Size 5.0 µm
5.0 µm
12% finer than
10 µm
10 µm
30% finer than
19 µm
19 µm
20 µm
20 µm
60% finer than
30 µm
30 µm
75% finer than
Particle Mesh Size 40 Mesh
40 Mesh
0% retained
100 Mesh
100 Mesh
0.1% retained
140 Mesh
140 Mesh
0.3% retained
170 Mesh
170 Mesh
0.4% retained
200 Mesh
200 Mesh
1.2% retained
325 Mesh
325 Mesh
10% retained
pH 8.2
8.2
Specific Surface Area 0.70 - 1.1 m²/g
0.70 - 1.1 m²/g
Component Elements Properties Metric English Comments
Al2O3 14 %
14 %
CaO 1.1 %
1.1 %
Fe2O3 0.060 %
0.060 %
K2O 2.8 %
2.8 %
Loss on Ignition(%) 0.30 %
0.30 %
Na2O 4.9 %
4.9 %
SiO2 76.8 %
76.8 %
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %