Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 200 °C |
27 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 200 °C |
27 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE) Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 200 °C |
27 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 0615 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 260 °C |
27 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Melt Flow | 27 - 39 g/10 min @Load 21.6 kg, Temperature 190 °C |
27 - 39 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 260 °C |
27 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Melt Flow | 27 - 39 g/10 min @Load 21.6 kg, Temperature 190 °C |
27 - 39 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 27 g/10 min @Load 21.6 kg, Temperature 190 °C |
27 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene EX1 is a high density polyethylene with 1-Butene as co monomer. It has acceptable tear strength, medium molar mass and narrow molar mass distribution.Applications: stretched film and tapes for prod.. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | 27 g/10 min @Load 21.6 kg, Temperature 190 °C |
27 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene EX2 (HF 7750) is high density polyethylene with propylene as co monomer. It has a medium molar mass with a narrow molar mass distribution.Application: production of monofilaments with high tensile.. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 265 °C |
27 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 250 °C |
27 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 265 °C |
27 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 250 °C |
27 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 230 °C |
27 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Melt Flow | 27 g/10 min @Load 21.6 kg, Temperature 190 °C |
27 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 29 H HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |