Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EX1 is a high density polyethylene with 1-Butene as co monomer. It has acceptable tear strength, medium molar mass and narrow molar mass distribution.Applications: stretched film and tapes for production of high strength knitted & wovens.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ISO 1183
Melt Flow 1.8 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
27 g/10 min

@Load 21.6 kg,
Temperature 190 °C
27 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Tensile Stress 32.0 MPa
4640 psi
at Break; ISO 527
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527
Elongation at Break >= 1000 %
>= 1000 %
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Tensile Modulus 0.800 GPa
116 ksi
ISO 527
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Softening Point 73.0 °C
163 °F
ISO 306
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Processing Properties Metric English Comments
Melt Temperature 200 - 280 °C
392 - 536 °F
Descriptive Properties Value Comments
Flexural Creep Modulus (MPa) 900
4 point, 1 min; DIN 19537-2
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved