Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Silicone Property; Arlon SQA-TMS-024
1.70 g/cc
0.0614 lb/in³
Laminated ETFE Film Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
ETFE Film; Arlon SQA-TMS-003
457 microns
18.0 mil
Side 1; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 18
18
Silicone Property; Arlon SQA-TMS-014
Hardness, Shore D 67
67
Laminated ETFE Film Property; Arlon SQA-TMS-014
Tensile Strength 6.89 MPa
1000 psi
Silicone Property; Arlon SQA-TMS-008
41.4 MPa
6000 psi
Laminated ETFE Film Property; Arlon SQA-TMS-008
Elongation at Break 300 %
300 %
Laminated ETFE Film Property; Arlon SQA-TMS-008
950 %
950 %
Silicone Property; Arlon SQA-TMS-008
Poissons Ratio 0.50
0.50
Silicone Property
Tear Strength 13.1 kN/m
75.0 pli
Silicone Property; Arlon SQA-TMS-029
Peel Strength 2.10 kN/m
12.0 pli
Ply-Adhesion; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; Arlon SQA-TMS-022
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Silicone Property; Arlon SQA-TMS-022
Maximum Service Temperature, Inert 154 °C
310 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
UL RTI, Electrical 65.6 °C
150 °F
File E54153
UL RTI, Mechanical without Impact 65.6 °C
150 °F
File E54153
Electrical Properties Metric English Comments
Dielectric Strength >= 41.42 kV/mm
>= 1052 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.103 - 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 15.0 - 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
Descriptive Properties Value Comments
Color Translucent
Total Product Weight (oz/yd2) 15.6
Arlon SQA-TMS-025
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved