Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave 1
76.2 microns
3.00 mil
Interleave 2
127 microns
5.00 mil
Side 1; Arlon SQA-TMS-003
127 microns
5.00 mil
Substrate; Arlon SQA-TMS-003
508 microns
20.0 mil
Side 2; Arlon SQA-TMS-003
762 microns
30.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
Silicone Property; ASTM D2240
Tensile Strength 8.853 MPa
1284 psi
Silicone Property; ASTM D412
Elongation at Break 449 %
449 %
Silicone Property; ASTM D412
Tear Strength 18.9 kN/m
108 pli
Die B, Silicone Property; ASTM D624
Peel Strength 4.58 kN/m
26.1 pli
Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test 1.5
1.5
[in], Char Length; FAR 25.853 App. F, P.1, S.Aii
8.0
8.0
[sec], Flame Time; FAR 25.853 App. F, P.1, S.Aii
Electrical Properties Metric English Comments
Dielectric Strength 31.9 kV/mm
811 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Blue
Interleave 2
Red
Red
Substrate
Total Product Weight (oz/yd2) 29
Arlon SQA-TMS-025